Ramesh, R and Ravikumar, K and Kishore, * (1986) Wear of En 31 steel. In: Transactions of the Indian Institute of Metals, 39 (4). pp. 329-334.
Full text not available from this repository. (Request a copy)Abstract
The microstructure effect on dry friction and wear of steel En 31 was evaluated by SEM, Rockwell C hardness, and dry sliding tests, using various heat treatments (full annealing, normalizing, water quenching, and spheroidizing). Full annealing resulted in max. wear loss whereas the martensitic structure had high wear resistance. A structure consisting of martensite, carbide, and retained austenite had the highest wear resistance. The dry wear in air was controlled by both oxidn. and wear mechanisms.
| Item Type: | Journal Article |
|---|---|
| Additional Information: | Copyright to this article belongs to Indian Institute of Metals |
| Keywords: | En 31 steel |
| Department/Centre: | Division of Mechanical Sciences > Materials Engineering (formerly Metallurgy) |
| Date Deposited: | 17 Jun 2008 |
| Last Modified: | 27 Aug 2008 13:28 |
| URI: | http://eprints.iisc.ernet.in/id/eprint/14393 |
Actions (login required)
![]() |
View Item |